Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 70.2 W/m-K
487 BTU-in/hr-ft²-°F
Special Metals Nickel 200
Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us..
Thermal Conductivity 70.2 W/m-K
487 BTU-in/hr-ft²-°F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Thermal Conductivity 70.2 W/m-K
487 BTU-in/hr-ft²-°F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..