Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1425 - 3410 °C | 2597 - 6170 °F | |
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |
|||
Melting Point | 1200 - 3410 °C | 2190 - 6170 °F | |
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Melting Point | 1200 - 3410 °C | 2190 - 6170 °F | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Melting Point | 1425 - 3410 °C | 2597 - 6170 °F | |
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Melting Point | 1425 - 3410 °C | 2597 - 6170 °F | |
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Melting Point | 1085 - 3410 °C | 1985 - 6170 °F | |
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11 Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc. |
|||
Melting Point | 1085 - 3410 °C | 1985 - 6170 °F | |
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10 Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc. |
|||
Melting Point | 1085 - 3410 °C | 1985 - 6170 °F | |
CMW® ELKONITE® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated Uses: Arcing and current carrying electrical contacts. Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated For electrical contacts resistant to arcing and welding in circuit breakers, etc.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 2140C Copper Tungsten Nickel material For structural rotors.Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material High wear resistance and reliability.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 30W3 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12 For projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members. Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 3W3 Tungsten Copper material ASTM B702 For arcing and current carrying electrical contacts, power transformer contacts, resistance welding electrodes.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 3W53 Heat Treatable Tungsten Copper material For resistance welding electrodes.Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 40W3 Infiltrated Tungsten Copper material ASTM B702 For vacuum switch contacts, low expansion structural members.Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 45S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Melting Point | 980 - 3410 °C | 1800 - 6170 °F | |
CMW® ELKONITE® 50S Infiltrated Tungsten Silver contact material ASTM B631, Class C, infiltrated For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 50W3 Tungsten Copper material ASTM B702 For vacuum switch contacts.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® ELKONITE® 5W3 Tungsten Copper material ASTM B702, Class C, infiltrated For arcing and current carrying electrical contacts; power transformer contacts.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® THERMKON® 62 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® THERMKON® 76 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Melting Point | 1425 - 3410 °C | 2597 - 6170 °F | |
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |