SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 280 °C
26 g/10 min

@Load 4.76 lb,
Temperature 536 °F
ASTM D1238
67 g/10 min

@Load 5.00 kg,
Temperature 280 °C
67 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 66 %
66 %
Type I, 50 mm/min; ASTM D638
Flexural Strength 93.0 MPa
13500 psi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
0.930 J/cm

@Temperature -30.0 °C
1.74 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 85.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 195 °C

@Thickness 6.40 mm
383 °F

@Thickness 0.252 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 22.4 kV/mm

@Thickness 1.60 mm
569 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.017

@Frequency 1.00e+6 Hz
0.017

@Frequency 1.00e+6 Hz
ASTM D150