Physical Properties Metric English Comments
Apparent Bulk Density 0.650 - 0.850 g/cc
0.0235 - 0.0307 lb/in³
ISO 60
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage  (discontinued **)&
Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak ..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin
Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that ..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that ..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade
Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade
Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
circa
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, 50% RH
Neat resin, for injection molding.Information provided by Cresset Powers Ltd.
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
circa
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, Dry As Molded
Neat resin, for injection molding.Information provided by Cresset Powers Ltd.
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
circa
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, 50% RH
Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd.
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
circa
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, Dry As Molded
Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd.
Apparent Bulk Density 0.650 - 0.720 g/cc
0.0235 - 0.0260 lb/in³
IS 867-1963
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Teknor Apex Sinvicomp DFR 5806 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Ashley Polymers Ashlene® R6043 Nylon 6
Medium viscosity extrusion grade Nylon 6 resin with excellent melt stability, good melt strength: suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, tou..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 60
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures  (discontinued **)
Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good ..
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc..
Copyright © lookpolymers.com All Rights Reserved