Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled , Polycarbonate, PTFE Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 54.5 MPa
7900 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.4 µm/m-°C
18.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Unannealed; ASTM D648
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257