Ashley Polymers Ashlene® 520-50G Nylon 66, 50% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 520-50G Nylon 66, 50% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% Glass reinforced Nylon 66.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 205 MPa
29700 psi
ATSM D638
Elongation at Break 2.0 %
2.0 %
Flexural Modulus 11.8 GPa
1710 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 252 °C
486 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648