Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM Data |
Americas Styrenics Styron® 484C High Impact Polystyrene
(discontinued **) STYRON® 484C high impact polystyrene resin, is typically used in refrigeration applications, appliances, containers, lids, furniture and profiles. It offers excellent low temperature toughness, exc.. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F; ASTM D648 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 6.35 mm |
2.40 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® LCP-30GF/000 Liquid Crystal Polymer - 30% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.40 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Multibase Multi-Flamâ„¢ 2318 PP Polypropylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingFurnitureInformation provided by Multibase |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific) LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF30 L X MT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: SilverTPCI# 7210102Information provid.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6,6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricatedFeatures: LubricatedProcessing Method: Injection MoldingAppearance: .. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC (Asia Pacific) LNP* Thermocomp* DX06410 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature -40.0 °C |
2.40 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Ensinger Hydex™ 301 Rigid Polyurethane (PU) Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature 22.8 °C |
2.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature 22.8 °C |
2.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436C10L Calcium Reinforced |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 212 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AEN 6000-2 Nylon 6 Engineered Resin |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |