Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87624 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 3.45 - 17.0 GPa | 500 - 2470 ksi | Average value: 8.25 GPa Grade Count:66 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
M. Holland Company SA400 Styrene Acrylonitrile High clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
Techmer ES HiFill FR® PC GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
(discontinued **) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |