Total PSI 945E Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name PSI
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSI 945E Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 945E is a high impact polystyrene designed for applications requiring extra toughness without sacrificing mechanical properties. Excellent falling dart impact combined with the high gloss. This polymer is superior for co-extrusion of high gloss sheet. 945E has unique capabilities for deep draw thermoforming with good sidewall distribution.An excellent candidate for ABS applications.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 43.4 MPa
6300 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Falling Dart Impact 18.07 J
13.33 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 88 %
88 %
60°; ASTM D523