Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 508 - 991 microns | 20.0 - 39.0 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubbe.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: MylarAppearance: Pink high viscosity gumThis data represents typical values for the production material. The data.. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: MylarAppearance: Pink high viscosity gumThis data represents typical values for the production material. The data.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 19540R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma.. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Thickness | 508 microns | 20.0 mil | Overall Rubber Thickness; Arlon SQA-TMS-012 |
Arlon 920-10Bxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201R##-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Desi.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon T3020-R004 0.020" (0.508 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76.. |
|||
Thickness | 508 microns | 20.0 mil | |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Thickness | 508 microns | 20.0 mil | ASTM D1000 |
3M Scotchrap™ 51 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31570R020 0.020" (0.508 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the pr.. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35232B020 0.020" (0.508 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Thickness | 508 microns | 20.0 mil | Overall |
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe.. |
|||
Thickness | 508 microns | 20.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R3781-920-##R##-P0 Silicone Rubber This fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tap.. |
|||
Thickness | 508 microns | 20.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |