Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
(discontinued **) Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubbe.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: MylarAppearance: Pink high viscosity gumThis data represents typical values for the production material. The data.. |
|||
Thickness | 508 microns | 20.0 mil | Silicone |
Arlon 41570R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51146R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness |
Arlon 51422R020 0.020" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and should no.. |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51866R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 920-10C##FR-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Thickness | 508 microns | 20.0 mil | Arlon SQA-TMS-003 |
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201B##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon LW201C##FR-P0 Silicone Rubber Triangular cross section of self-fusing silicone tape. Interleave: 3 mil PE. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Thickness | 508 microns | 20.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51106R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness |
Arlon 51921R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production .. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201C##FR-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 20 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indica.. |
|||
Thickness | >= 508 microns | >= 20.0 mil | Side 2 |
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 508 microns | 20.0 mil | Silicone |
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44430B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassProduct Use: Belting materialAppearance: Black colored high viscosity gum on fiberglass fa.. |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R3792-920-10R##-P0 Silicone Rubber This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38726R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeProduct Use: Flexible heater substrateAppearance: Red colored, high .. |
|||
Thickness | 508 - 787 microns | 20.0 - 31.0 mil | Range of Thicknesses Available |
Rogers Corporation Bisco® EC-2040 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.020 inches and 0.031 inchesInformation provided by Rogers Corporation. |