Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A3015-R004-12 0.015" (0.381 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Transverse Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412 |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | |
Teknor Apex Tekbond® TB 1372A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | |
Teknor Apex Tekbond® TB 1415A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | |
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P2 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Certified to meet all requirements of US Military Specification A-A5.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; Arlon SQA-TMS-009 |
Arlon 920-10Hxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.D.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 920-10R##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 920-10T##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Transparent, Rectangular cross-section, S.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Tape Property; ASTM D412 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW201R##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW401B##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW401B##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW50125Rxx-P0 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Se.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-20R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 2” Wide Rectangular 2 inch wide, 15 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW401B##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |