Mechanical Properties Metric English Comments
Tensile Strength 23.1 MPa
3350 psi
Product Property; Arlon SQA-TMS-048
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  
1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod..