Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 47568R0055E 0.0075" (0.190 mm) Cured Silicone Rubber/Acrylic PSA

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 47568R0055E 0.0075" (0.190 mm) Cured Silicone Rubber/Acrylic PSA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 2113 FiberglassSide 2: Acrylic PSA Interleave: Polypropylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
50.8 microns
2.00 mil
Side 2; Arlon SQA-TMS-003
88.9 microns
3.50 mil
Substrate; Arlon SQA-TMS-003
191 microns
7.50 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Silicone Property; ASTM D412
Elongation at Break 600 %
600 %
Silicone Property; ASTM D412
Peel Strength 0.0877 kN/m
0.500 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Red
Substrate
Total Product Weight (oz/yd2) 6.5
Arlon SQA-TMS-025