Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.21 MPa | 900 psi | Typical |
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | |
Shin-Etsu Silicones KEG-2000-20A/B Elastomer KEG-2000-20 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Silicone Property |
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Silicone Property |
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1 Silicone Property; ASTM D412 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2 Silicone Property; ASTM D412 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Compound Property |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon CP-322 Bulk Compound Product Use: Silicone rubber (bulk compound)Appearance: Red silicone rubber.This data represents typical values for the production material. The data should not be used to write, or in place of, mat.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon R32089R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon R34381R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 7628 Style FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typical.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon R35782R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 FiberglassThis data represents typical values for the production mat.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Compound Property; ASTM D412 |
Arlon 31570R020 0.020" (0.508 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the pr.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Silicone Property |
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51426W015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon R32458R0055E 0.0075" Cured Silicone Rubber with Fiberglass Substrate and Acrylic PSA Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Acrylic PSAInterleave: PolypropyleneThis data represents typical values for the production material and sh.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 44602M020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance Tan rubber on glass fiber fabricThis data represents typical values for the production material. The data should not be used to write, or .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the produ.. |