Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.21 MPa | 900 psi | Typical |
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Tensile Strength | 6.21 MPa | 901 psi | BAM 1211 |
Kraton® G1651 H (SEBS) Linear Triblock Copolymer Description: Kraton G1651 H is a clear, linear copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | |
Shin-Etsu Silicones KEG-2000-20A/B Elastomer KEG-2000-20 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy.. |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
900 psi @Strain 100 % |
ASTM D638 |
Teknor Apex APEX® 3300-75NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Food Service Application; Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tek.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Compound Property |
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Silicone Property |
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 28601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Product Use: Flexible Heater InsulationAppearance: White silicone gum on fiberglass with polymer release linersThis.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51422R020 0.020" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and should no.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51571R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene Appearance: Black silicone gum on fiberglass clothThis da.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon CP-322 Bulk Compound Product Use: Silicone rubber (bulk compound)Appearance: Red silicone rubber.This data represents typical values for the production material. The data should not be used to write, or in place of, mat.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon CP-PC-2959 Silicone Product Use: Traction motor insulation compound, electrical insulationAppearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to writ.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580XC015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Silicone Property |
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon R33216R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property, Side 1; ASTM D412 |
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 47568R0055E 0.0075" (0.190 mm) Cured Silicone Rubber/Acrylic PSA Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 2113 FiberglassSide 2: Acrylic PSA Interleave: Polypropylene This data represents typical values for the production material. The.. |