Material Notes:
Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applications where explosive decompression may occur. Suitable for use with sour (H2S) crude oil and gas, which may also include lubricating, oil additives and amine corrosion inhibitors. High mechanical strength and excellent chemical resistance.
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
°IRHD; ASTM D1415
91
91
°IRHD, +2 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 32.1 MPa
4660 psi
ASTM D412
33.22 MPa
4819 psi
3.5% change after 70 hours @ 150°C; ASTM D412
Elongation at Break 264 %
264 %
ASTM D412
273.24 %
273.24 %
3.5% change after 70 hours @ 150°C; ASTM D412
Compression Set 20 %
20 %
22 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
-25.0 °C
-13.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F