Material Notes:
Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No need of lubricant. Low friction coefficient. High density (d=4). Outstanding compressive strength. High thermal conductivity. High dimensional stability (low moisture absorption).Example applications: Auto-lubricating bearing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 3.80 g/cc
0.137 lb/in³
Water Absorption 0.30 %
0.30 %
Melt Flow 17.7 g/10 min

@Load 5.00 kg,
Temperature 235 °C
17.7 g/10 min

@Load 11.0 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.0 MPa
6090 psi
5 mm/min
Elongation at Break 2.0 %
2.0 %
5 mm/min
Tensile Modulus 4.97 GPa
721 ksi
1 mm/min
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in