Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 183 °C | 361 °F | |
Omnia Plastica PA 11 Rilsan B The only engineering plastic of natural origin (derived from castor oil), it is a polyamide which, unlike the other nylons, does not absorb humidity. It has all the good mechanical features of polya.. |
|||
Melting Point | 183 °C | 361 °F | DSC, both heating and cooling speeds of 10°C/min |
Noltex Soarnol® DC3203F Ethylene Vinyl Alcohol Copolymer Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%.Information provided by Soarus, LLC. In the Un.. |
|||
Melting Point | 183 °C | 361 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n.. |
|||
Melting Point | 183 °C | 361 °F | DSC |
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat.. |
|||
Melting Point | 183 - 257 °C | 361 - 495 °F | |
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 268 °C | 361 - 514 °F | |
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 288 °C | 361 - 550 °F | |
Indium Corp. Indalloy 153 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 °C | 361 °F | Eutectic |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 183 - 238 °C | 361 - 460 °F | |
Johnson Matthey JM4060 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 °C | 361 °F | |
Johnson Matthey JM6337 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 - 288 °C | 361 - 550 °F | |
Williams Advanced Alloys WS288 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 °C | 361 °F | |
Goodfellow Tin 60/Lead 39/Antimony 1 Alloy A general purpose, low melting point soft solder which can also be used as a protective coating and for metal film capacitors.Information provided by Goodfellow. |
|||
Melting Point | 183 °C | 361 °F | DIN 53 736 |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned) Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier .. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMF Nylon 11 (Dry) Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMN D Nylon 11 (Dry) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMV Nylon 11 (Dry) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® MB 3750 Nylon 11, Transparent Grade (Dry) Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Dry) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® MB 3750 Nylon 11, Transparent Grade (Conditioned) Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical.. |
|||
Melting Point | 183 - 190 °C | 361 - 374 °F | |
Johnson Matthey JM6040 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Conditioned) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |
|||
Melting Point | 183 °C | 361 °F | DSC |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |