Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.7 g/10 min @Load 2.16 kg, Temperature 300 °C |
17.7 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HM3020H PPE+PS (Asia Pacific) PPE+PS GF+MF 30% filled, FR V-1, high flow |
|||
Melt Flow | 17.7 g/10 min @Load 5.00 kg, Temperature 235 °C |
17.7 g/10 min @Load 11.0 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Melt Flow | 17.7 g/10 min @Load 5.00 kg, Temperature 235 °C |
17.7 g/10 min @Load 11.0 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |