Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.73e+12 ohm | 2.73e+12 ohm | |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |