Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.80 MPa
261 psi
ISO 37
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-..
Tensile Strength, Yield 1.80 MPa
261 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7284 Butyl and Halobutyl Rubber
Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.80 MPa
261 psi
ASTM D638
Arkema Group OREVAC® 9305 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Tensile Strength, Yield 1.80 MPa

@Strain 50.0 %
261 psi

@Strain 50.0 %
50 mm/min
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Tensile Strength, Yield 1.80 MPa

@Strain 50.0 %
261 psi

@Strain 50.0 %
50 mm/min
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Tensile Strength, Yield 1.80 - 34.0 MPa
261 - 4930 psi
Average value: 14.0 MPa Grade Count:39
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Yield 1.80 - 70.0 MPa
261 - 10200 psi
Average value: 14.2 MPa Grade Count:104
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade