Axiall 8264 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8264 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. Printable film and picture album pages are examples of its many uses. Electronic packaging and transistor magazine profiles are produced using 8624. It is also suitable for box lid applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 44.1 MPa
6400 psi
ASTM D-638
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Flexural Strength 77.2 MPa
11200 psi
ASTM D-790
Flexural Modulus 2.65 GPa
385 ksi
ASTM D-790
Izod Impact, Notched 1.98 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.70 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
5.23 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 187 kJ/m²
89.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.049 inch(min. thickness)
Optical Properties Metric English Comments
Haze 5.0 %

@Thickness 3.17 mm
5.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 75 %

@Thickness 3.17 mm
75 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Cell Classification 13353
ASTM D-1784