Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax CCP PBT 1100-630S Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax PBT 1100-211S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika AX-1500W Conditioned Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Cast Film |
Arkema Group Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |