Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 8 - 10 hour | 8 - 10 hour | Demold time, catalyzed with Moldmaster Purple |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Dry Time | 8 - 12 hour | 8 - 12 hour | Demold time, catalyzed with QM 260B |
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica Castable ceramic with low thermal conductivity. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina Fine grain castable ceramic. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate High Density, high strength molding compound. |
|||
Dry Time | 8 - 12 hour | 8 - 12 hour | Hard |
Abatron MasterMold 12-3 Flexible Mold Making Compound Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surf.. |