Mechanical Properties Metric English Comments
Compressive Strength 70.0 - 90.0 MPa
10200 - 13100 psi
ISO 604
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Compressive Strength 70.0 - 90.0 MPa
10200 - 13100 psi
ISO 604
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Compressive Strength 70.0 MPa
10200 psi
Cold Crushing Strength
Gouda Vuurvast AK 60 A Dense Refractory Brick
Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% ..
Compressive Strength 70.0 MPa
10200 psi
Cold Crushing Strength
Gouda Vuurvast AK 80 A Dense Refractory Brick
Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s..
Compressive Strength 70.0 MPa
10200 psi
Cold Crushing Strength
Gouda Vuurvast AK 80 AP Dense Refractory Brick
Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks..
Compressive Strength 70.0 MPa
10200 psi
Cold Crushing Strength
Gouda Vuurvast AK 82 A Dense Refractory Brick
Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa..
Compressive Strength 70.0 MPa
10200 psi
Cold Crushing Strength
Gouda Vuurvast AK 98 Dense Refractory Brick
Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette..
Compressive Strength 70.0 MPa

@Time 3.60e+7 sec
10200 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..
Compressive Strength 70.0 MPa
10200 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Compressive Strength 70.3 MPa
10200 psi
Tra-Con Tra-Bond FS12 Fast Cure Epoxy Adhesive System
TRA-BOND FS12 is an epoxy resin formulation developed for room temperature bonding applications where a fast cure epoxy adhesive is needed. This effective epoxy formulation consists of 100% reactive..
Compressive Strength >= 70.0 MPa
>= 10200 psi
Axial; IEC 1212-2 4.2
Hippe PF CP 31 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity.Information provided by Hippe.
Compressive Strength 70.3 MPa
10200 psi
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina
Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic..
Compressive Strength 70.0 MPa

@Temperature 200 °C
10200 psi

@Temperature 392 °F
EN ISO 604
Brandenburger S 2000 A Side Insulation
S 2000 A is reinforced with load-bearing glass fibre mat with thermoset weave. A laminated aluminum lining provides additional heat-reflecting protection.Information provided by Brandenburger Isolie..
Copyright © lookpolymers.com All Rights Reserved