Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 60 - 120 min | 60 - 120 min | |
NextGen Adhesives P907-13 Fiber Optic Adhesive Description: NGAC P907-13 is a rapid curing, low viscosity, heat cured epoxy adhesive system that is specifically formulated for use in the fiber optic industry.Advantages and Applications: Uses inc.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Mass: 100g |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Pot Life | 120 - 120 min @Temperature 80.0 - 80.0 °C |
120 - 120 min @Temperature 176 - 176 °F |
Average value: 120 min Grade Count:1 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Time before parts must be mated |
Lord Adhesives 304 General Purpose, High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Time before parts must be mated |
Lord Adhesives 305 General Purpose, Medium Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Time before parts must be mated |
Lord Adhesives 306 High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Time before parts must be mated |
Lord Adhesives 307 General Purpose, Medium Viscosity Hardener for Lord 305-1 Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Time before parts must be mated |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 90 - 120 min @Temperature 25.0 °C |
90 - 120 min @Temperature 77.0 °F |
54g mass |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21NDFG Two component epoxy compound for high performance applications Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Epoxy Technology EPO-TEK® 301-1 Optical Grade Epoxy Material Description: A two component, room temperature curing, optical grade epoxy, designed for optics, medical, and opto-electronic packaging of semiconductor devices, components, and electronics.. |
|||
Pot Life | 60.0 - 120 min | 60.0 - 120 min | |
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing. |
|||
Pot Life | 60.0 - 120 min | 60.0 - 120 min | |
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide Single-part castable ceramic exhibiting high strength and thermal conductivity. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 20.0 - 120 min | 20.0 - 120 min | Average value: 92.2 min Grade Count:9 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Pot Life | 75 - 120 min | 75 - 120 min | 100 gram batch |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |
|||
Pot Life | 2.00 - 120 min | 2.00 - 120 min | Average value: 28.2 min Grade Count:21 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |