Physical Properties Metric English Comments
Density 1.76 - 1.95 g/cc
0.0636 - 0.0704 lb/in³
Pyrotek Dense Fused Silica Pre-Cast Shapes
Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe..
Density 1.90 - 1.95 g/cc
0.0686 - 0.0704 lb/in³
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed...
Density 1.80 - 1.95 g/cc
0.0650 - 0.0704 lb/in³
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 1.85 - 1.95 g/cc
0.0668 - 0.0704 lb/in³
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 1.75 - 1.95 g/cc
0.0632 - 0.0704 lb/in³
Molded
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound
BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps..
Density 1.75 - 1.95 g/cc
0.0632 - 0.0704 lb/in³
Molded
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap..
Density 1.90 - 1.95 g/cc
0.0686 - 0.0704 lb/in³
Pyrotek Pyrocast XL Small Component Refractory
ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast..
Density 1.03 - 1.95 g/cc
0.0372 - 0.0704 lb/in³
Average value: 1.72 g/cc Grade Count:31