Thermal Properties Metric English Comments
CTE, linear 7.74 µm/m-°C

@Temperature 20.0 °C
4.30 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 200 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
CTE, linear 7.74 µm/m-°C

@Temperature 20.0 °C
4.30 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 201 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
CTE, linear 7.74 µm/m-°C
4.30 µin/in-°F
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.74 µm/m-°C
4.30 µin/in-°F
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.74 µm/m-°C
4.30 µin/in-°F
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.74 µm/m-°C

@Temperature 20.0 °C
4.30 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina
Fine grain castable for potting and producing small tools.