Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.74 µm/m-°C @Temperature 20.0 °C |
4.30 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
CTE, linear | 7.74 µm/m-°C @Temperature 20.0 °C |
4.30 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
CTE, linear | 7.74 µm/m-°C | 4.30 µin/in-°F | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.74 µm/m-°C | 4.30 µin/in-°F | |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.74 µm/m-°C | 4.30 µin/in-°F | |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.74 µm/m-°C @Temperature 20.0 °C |
4.30 µin/in-°F @Temperature 68.0 °F |
|
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |