Albis Plastics PC/PET 361E Unfilled  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics PC/PET 361E Unfilled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and Automotive ApplicationsProcessing: Injection Molding: Melt Temperature:530-550° F, Mold Temperature:130-160° FData supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.3 MPa
8750 psi
ASTM D638
Tensile Strength, Yield 61.7 MPa
8950 psi
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.29 GPa
332 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
1/8" sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 277 - 288 °C
531 - 550 °F
Injection
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F