Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
NYCOA 2084 HS Super-Tough, High Viscosity Nylon 6 Resin NYCOA 2084 HS is a high viscosity resin particularly suitable for extrusion processing. Its melt viscosity and strength provide ease of processing for tubing, profile, and molded articles. This mate.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® AD143 PC (Asia Pacific) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East) IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® IR2240 PC (Europe-Africa-Middle East) IR 2240 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | natural, tints; ASTM D256 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 955A PC Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
RTP Company PermaStat® 1800A FR UV Polycarbonate/Acrylic Alloy (PC/PMMA) Anti-Static - Flame Retardant - UV Stable Anti-Static - Flame Retardant - UV StableComments:Permanently Anti-StaticESD ProtectionFlame RetardantUV StabilizedUnless otherwise specified, all data listed is for natural or black colored materia.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1003R PC (Asia Pacific) PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R6000 FR-PC Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.20 mm |
15.0 ft-lb/in @Thickness 0.126 in |
ASTM D 256 |
RTP Company RTP 2000 HC A Polyester Alloy Medical Cleaner Resistant - UV Stabilized RTP 2000 HC series are polyester alloys designed to withstand the aggressive cleaners used to disinfect medical equipment |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1310L1 HB Polycarbonate Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 22.8 °C |
15.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA2SP0003 Nylon 6, High Gloss Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Adell DS-10 General Purpose Polycarbonate |
|||
Izod Impact, Notched | >= 8.00 J/cm | >= 15.0 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.20 mm |
15.0 ft-lb/in @Thickness 0.126 in |
ASTM D 256 |
RTP Company RTP 399 X 86846 H Polycarbonate (PC) Flame Retardant - Halogen Free - Transparent |