Mechanical Properties Metric English Comments
Flexural Modulus 2.29 GPa
332 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Flexural Modulus 2.29 GPa
332 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Flexural Modulus 2.29 GPa
332 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East)
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Flexural Modulus 2.29 GPa
332 ksi
ASTM D790
Albis Plastics PC/PET 361E Unfilled  (discontinued **)
Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and..
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC
LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare
Flexural Modulus 2.29 GPa
332 ksi
(102 mm Span) 3mm/min; ASTM D790
LNP ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant  (discontinued **)
Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500.Features: Lubricated, Good Wear ResistanceForms: PelletsInformation provided by LNP, a GE Plasti..
Flexural Modulus 2.29 GPa

@Thickness 3.20 mm
333 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro..
Flexural Modulus 2.29 GPa
332 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS
LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant.
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Flexural Modulus 2.29 GPa
332 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® X6125 PBT+PC
Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.29 GPa
332 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp DX93681 PC
LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.29 GPa
332 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp DX93681 PC (Asia Pacific)
LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.29 GPa
333 ksi
ASTM D790
Samyang Trimma® SD6350H PMMA, Opaque
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PVX524 PPE
PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT