Polymer Property : Izod Impact, Notched = 8.01 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Multibase Nylex™ 1230 Polyamide + PP
Forms: PelletsInformation provided by Multibase
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific)
Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 945 PC
Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm
15.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Ravago Manufacturing Americas Hylex® P1310L Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release
Information provided by Entec.
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXE144H PC
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
natural, tints; ASTM D256
SABIC Innovative Plastics Lexan® HP4R PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
natural, tints; ASTM D256
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East)
Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction.
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
1/8" sample; ASTM D256
Albis Plastics PC/PET 361E Unfilled  (discontinued **)
Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 141 PC
General purpose polycarbonate with melt flow rate of 10.5.
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific)
10.5 MFR. UV-stabilized. Improved flame retardance.
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific)
Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 945U PC (Asia Pacific)
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 955U PC (Asia Pacific)
Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo..
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HP4 PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp DX99854 PC (Asia Pacific)
LNP* LUBRICOMP* DX99854 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.This data was supplied by SABIC-I..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd..
Izod Impact, Notched 8.01 J/cm

@Temperature 22.8 °C
15.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded
V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc.