Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatures as well as easy processing. AKROMID® A is an engineering plastic compound that allows a broad range of possible applications. On the basis of these standard types, we are able to develop individual compounds for special application needs.Information from Akro-Plastic
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Filler Content 30 %
30 %
ISO 1172
Water Absorption 1.9 - 2.1 %

@Temperature 70.0 °C
1.9 - 2.1 %

@Temperature 158 °F
62% r.h., Humidity; ISO 62
Water Absorption at Saturation 5.2 - 5.8 %

@Time 82800 sec
5.2 - 5.8 %

@Time 23.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
5 [mm/min]; ISO 527-1/2
Elongation at Break 5.5 %
5.5 %
5 [mm/min]; ISO 527-1/2
Tensile Modulus 7.10 GPa
1030 ksi
1[mm/min]; ISO 527-1/2
Flexural Strength 220 MPa
31900 psi
2 [mm/min]; ISO 178
Flexural Modulus 7.20 GPa
1040 ksi
2 [mm/min]; ISO 178
Charpy Impact Unnotched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357-1/3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved