Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories CRAG-S50 Long Stopper

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CRAG-S50 Long Stopper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.58 g/cc
0.0932 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.006867 GPa

@Temperature 1400 °C
0.9960 ksi

@Temperature 2550 °F
0.0079461 GPa

@Temperature 23.0 °C
1.1525 ksi

@Temperature 73.4 °F
Compressive Strength 29.4 MPa
4270 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.00 µm/m-°C

@Temperature 1000 °C
2.22 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 72 %
72 %
SiO2 2.0 %
2.0 %
Descriptive Properties Value Comments
Chemical Analysis(%),FC+SiC 23+2
Remarks High Corrosion resistance
Users viewing this material also viewed the following: