Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
Melt Index of Compound 13 - 19 g/10 min

@Temperature 230 °C
13 - 19 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 - 27.0 MPa
3480 - 3920 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Modulus 1.518 GPa
220.2 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256