Polymer Property : Specific Gravity = 1.06 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® FiberMax® 105B Strength enhancing fiber treatment
Description: Strength enhancing fiber treatmentUsage: FibreMax® 105B is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready, fiber treatment that increases th..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® Licomer® A 11 Acrylic polymer dispersion
Licomer® A 11 is an aqueous polymer dispersion suitable for the manufacture of products for the finishing of shoes and leather. This product provides excellent gloss and flexibility, and provides..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® Licomer® A 623 Styrene - Acrylate copolymer dispersion
Description: Styrene - Acrylate copolymer dispersionUsage: Licomer® A 623 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. ..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® Licomer® A 65 Styrene - Acrylate copolymer dispersion
Description: Styrene - Acrylate copolymer dispersionUsage: Licomer® A 65 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. T..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® Michem® Dispersion 91530 Acrylic resin dispersion
Michem® Dispersion 91530 is an additive used as a leveling aid, gloss enhancer and for buffability and mar resistance for the floor finish industry. This product is also effective for gloss enhan..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® Nomar® 70AFN Non-abrasive paper coating
Description: Non-abrasive paper coatingUsage: Nomar® 70AFN is a water based, gluable, non-abrasive coating generally used to provide abrasion protection for gas flushed food packaging or small ap..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® SofTak® 317 Non-skid coating
Description: Non-skid coating.Usage: SofTak® 317 is a gluable nonskid coating with excellent angle of skid. These properties are useful for slip or tier sheets, or a variety of other applications..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® SofTak® 326 Non-skid coating
Description: Non-skid coating.Usage: SofTak® 326 is an excellent nonskid coating that also has a fair amount of water resistance. It is often used on slip/tier sheets or a variety of other applic..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® SofTak® 734 Antiskid and soft feeling touch coating
Description: Antiskid and soft feeling touch coatingUsage: SofTak® 734 is an antislip coating for paper and board with a "leather-like" feel.Application Data: SofTak® 734 is rod, blade and fle..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® SofTak® 1637 Non-skid coating
Description: Non-skid coating.Usage: SofTak® 1637 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather-like" feel. This product is..
Specific Gravity 1.01 - 1.06 g/cc
1.01 - 1.06 g/cc
ASTM D792
Spartech Royalite R84/21 Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
Buckeye Polymers BP RPP 2008 T NAT Polypropylene, Talc Filled
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and ..
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
Buckeye Polymers BP RPP 2010 T NAT Polypropylene, Talc Filled
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and ..
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Michelman® StaticBan® 1005N Heat resistant conductive coating
Heat resistant conductive coatingUsage: StaticBan® 1005N is a conductive coating which imparts a reliable, electrically conductive surface around sensitive electronic parts such as integrated circu..