Polymer Property : Melt Index of Compound = 13 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polykemi AB POLYform POM C M140 Polyoxymethylene
Information provided by Polykemi AB
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY HRA222 ASA (Asia Pacific)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance.
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 260 °C
13 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Europe-Africa-Middle East)
Cycoloy Medium Heat Plating Grade for Automotive
Melt Index of Compound 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® 925 PC (Europe-Africa-Middle East)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
Melt Index of Compound 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® 925A PC (Europe-Africa-Middle East)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
Melt Index of Compound 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
Melt Index of Compound 13 - 16 g/10 min

@Load 21.6 kg,
Temperature 300 °C
13 - 16 g/10 min

@Load 47.6 lb,
Temperature 572 °F
cm³/10min; ISO 1133
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 220 °C
13 g/10 min

@Load 11.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM 1000RV PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 340 °C
13 g/10 min

@Load 11.0 lb,
Temperature 644 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 360 °C
13 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East)
PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 220 °C
13 g/10 min

@Load 11.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 220 °C
13 g/10 min

@Load 11.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 250 °C
13 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 420HP PBT
30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420..
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 250 °C
13 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 250 °C
13 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 250 °C
13 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 250 °C
13 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 265 °C
13 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East)
NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications.
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 280 °C
13 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade.
Melt Index of Compound 13 g/10 min

@Load 1.20 kg,
Temperature 280 °C
13 g/10 min

@Load 2.65 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness.
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 360 °C
13 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant.
Melt Index of Compound 13 g/10 min

@Load 10.0 kg,
Temperature 280 °C
13 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 260 °C
13 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific)
Cycoloy Medium Heat Plating Grade for Automotive