Polymer Property : Izod Impact, Unnotched = 9.29 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.96 J/cm

@Temperature 23.0 °C
9.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific)
LNP* Lubricomp* ZP001XXP is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
Izod Impact, Unnotched 4.96 J/cm

@Temperature -30.0 °C
9.29 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA
High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors.
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 621 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.