A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 50.0 MPa
7250 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.10 J/cm
13.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
244 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F