Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.10 J/cm @Thickness 3.18 mm |
13.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® EFL-4036 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Unnotched | 7.11 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu.. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 432 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 7.10 J/cm | 13.3 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 7.08 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact. |
|||
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |