Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C
444 - 475 °F
Copyright © lookpolymers.com All Rights Reserved