Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | ISO 75, ASTM D648 |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | ASTM D648 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C @Thickness 3.20 mm |
333 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | 0.125";; ASTM D648 |
Diamond Polymers NPP 60-1010 PCTA Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |