Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 167 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
ISO 75, ASTM D648
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
ASTM D648
BASF Capron® 8224 HSL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11
LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11
LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C

@Thickness 3.20 mm
333 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
332 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
0.125";; ASTM D648
Diamond Polymers NPP 60-1010 PCTA Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 167 °C
333 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved