Polymer Property : Tensile Strength, Ultimate = 10700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 73.8 MPa
10700 psi
ASTM D638
Nylene® Norpex® AX10GF , 10% Glass Reinforced Polyphenylene Ether
Description: Norpex® AX10GF is a 10% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric..
Tensile Strength, Ultimate 73.8 MPa
10700 psi
ASTM D638
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether
Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res..
Tensile Strength, Ultimate 73.5 MPa
10700 psi
ISO 527
Polikim KESTOIL® Polyamide 6 + Lubricant
Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ISO 527-2
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Tensile Strength, Ultimate 73.5 MPa
10700 psi
ISO 527
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an..
Tensile Strength, Ultimate 73.5 MPa
10700 psi
ASTM D638
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
10%/min; ASTM D638
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa..
Tensile Strength, Ultimate 73.77 MPa
10700 psi
Abatron AboCast 8-12/Abocure 8-12 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F..
Tensile Strength, Ultimate 73.5 MPa
10700 psi
DIN 53455; ASTM D638
Kolon KOPA® KN177N Nylon Extrusion Resin
Excellent transparent & flexible copolyamide, typical applications are fishing nets & fishing linesInformation provided by US distributor, API-Kolon.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Lucky IH-830 Acrylic, Injection Grade
Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent..
Tensile Strength, Ultimate 74.0 MPa

@Temperature 1093 °C
10700 psi

@Temperature 1999 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 73.5 MPa
10700 psi
DIN 53455; ASTM D638
Kolon KOPA® KN133G8ST Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Lucky CH-910 Acrylic, Coextrusion Grade
Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Plenco 1510 Polyester, Pellet, Injection Molded
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file ..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Plenco 6582 Phenolic, Briquette, Transfer Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade
Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ISO 527-2/1A/5
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Tensile Strength, Ultimate 74.0 MPa

@Temperature 982 °C
10700 psi

@Temperature 1800 °F
ASTM E8
ATI Allegheny Ludlum 309S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ATSM D638
Ashley Polymers Ashlene® P291WO PPO
A reinforced, flame retardant resin with outstanding structural strength. Good appearance and high impact.Data provided by the manufacturer
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Lucky EH-910 Acrylic, Extrusion Grade
Highest heat and stress cracking resistance of Lucky PMMA grades. Recommended for extrusion of sheets, pipes, and profiles. Can also be used for injection molding of small parts. May be UV stabil..