3M Scotchcast™ 2136 Potting Kit

Category Other Engineering Material
Manufacturer 3M
Trade Name Scotchcast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 2136 Potting Kit.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulating the 8 AWG ground connection in a wet-niche shell as required by NEC when using rigid, non-metallic conduit in the installation of wet-niche underwater lighting fixtures. Scotch cast 2136 compound is UL Listed as a potting compound for swimming pool, fountain or spa equipment and is for use only where adhering to copper, copper alloy and stainless steel materials.Information provided by 3M
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Polyol [Part B]; ASTM D891
1.018 g/cc
0.03678 lb/in³
ASTM D891
1.02 g/cc
0.0368 lb/in³
Mixed; ASTM D891
1.077 g/cc
0.03891 lb/in³
Prepolymer [Part A]; ASTM D891
Viscosity 770 cP
770 cP
Prepolymer [Part A]; 3M Method TM-173
1694 cP
1694 cP
Polyol [Part B]; 3M Method TM-173
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength at Break 6.43 MPa
933 psi
20'/min; ASTM D412
Elongation at Break 418 %
418 %
20'/min; ASTM D412
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -80.0 °C
-112 °F
Electrical Properties Metric English Comments
Dielectric Strength 12.5 kV/mm
318 kV/in
after 7 days 100°C; ASTM D149
13.1 kV/mm
334 kV/in
ASTM D149
Descriptive Properties Value Comments
Appearance Black
Polyol [Part B]
Black
Mixed
Pale to Clear
Prepolymer [Part A]