Polymer Property : Dielectric Strength = 334 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.1 kV/mm
334 kV/in
ASTM D149
3M Scotchcast™ 2136 Potting Kit
The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat..