Polymer Property : Tensile Strength at Break = 933 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.43 MPa
933 psi
20'/min; ASTM D412
3M Scotchcast™ 2136 Potting Kit
The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat..