Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.43 MPa | 933 psi | 20'/min; ASTM D412 |
3M Scotchcast™ 2136 Potting Kit The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat.. |